Convex, concave die gap between the control
and adjustment of the method
Convex, concave die clearance control, should according to die
structure, Precision stamping parts clearance size, blanking
pieces of quality and practical assembly condition to selected. Convex, concave
die gap between the control and adjustment method have the following kinds.
(1)Pervious to light
method
Will
convex, concave die after molmerged, shone a light on the underside, observe
the convex, concave die around through light and distribution to judge the size
of the clearance and uniformity. If not even, to adjust to evenly between fixed
again, this method is suitable for small gap plate stamping die.
(2)Feeler method
Will convex, concave die after molmerged, convex, concave die into the
thickness of unilateral clearance feeler convex, concave die gaps in each direction.
Precisionstamping parts Then tighten
the screw on mode. Finally put paper to stamping and will last mould seat and
fixed on board with drilling, reaming positioning pin hole, and at a pin
location.
(3)Gaskets DiaoZhengFa
Gasket adjustment method is simple, convenient, clearance is used
widely. As shown in figure 1 shows, the mat with good contour mat iron, will
gaskets wrapped in the punch to the punch into the concave mould, observe the
convex, concave die clearance condition. If clearance does not even, with
striking the protruding models of fixed plate method clearance adjustment, then
tighten the screw on mode. Finally put paper to stamping, observation on paper
cutting around burr and even rate to judge whether clearance convex, concave
die even, to adjust the gap until cutting burr uniform so far. Finally the
mould seat and the plate with drilling, reaming positioning pin hole, and enter
the pin location. This method widely used cutting materials focusing thick
large clearance and bending stamping, deep drawing mould clearance control.
(4)
Chemical method
When the convex, concave die complex shape, the use of the above several
methods more difficult to adjust the gap, the chemical method can be used to
control the gap, the plating method is used. Plating method is the punch in the
work surface coated with copper or zinc instead of washers. The plating
thickness and unilateral gap is same, Precisionstamping parts blade people concave die hole, and check the move without
block phenomenon can assembly tighten. Coating in use process will die fall off
naturally, need not removed. This uniform coating, can improve the uniformity
of assembling clearance.